Aluminum Alloy Castings: Properties, Processes, and Applications
Data Set 1: Aging Response Curves
-
Published:2004
Abstract
This data set presents aging response curves for a wide range of aluminum casting alloys. The aging response curves are of two types: room-temperature, or "natural," curves and artificial, or "high-temperature," curves. The curves in each group are presented in the numeric sequence of the casting alloy designation. The curves included are the results of measurements on individual lots considered representative of the respective alloys and tempers. The properties considered are yield strength, ultimate tensile strength, elongation, and Brinell hardness.
Aging Response Curves, Aluminum Alloy Castings: Properties, Processes, and Applications, By J. Gilbert Kaufman, Elwin L. Rooy, ASM International, 2004, p 133–173, https://doi.org/10.31399/asm.tb.aacppa.t51140133
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.