Aluminum Alloy Castings: Properties, Processes, and Applications
Chapter 8: Properties and Performance of Aluminum Castings
-
Published:2004
Abstract
This chapter reviews and provides data tables for the wide range of properties and performance characteristics that are possible with specific aluminum casting alloys and tempers. Properties and performance attributes addressed include casting and finishing characteristics; typical physical properties; typical and minimum (design) mechanical properties; fatigue strength; fracture resistance, including subcritical crack growth; and resistance to general corrosion and to stress-corrosion cracking. The chapter concludes with information on the properties of cast aluminum matrix composites.
Sign in
ASM members
Member Sign InProperties and Performance of Aluminum Castings, Aluminum Alloy Castings: Properties, Processes, and Applications, By J. Gilbert Kaufman, Elwin L. Rooy, ASM International, 2004, p 69–131, https://doi.org/10.31399/asm.tb.aacppa.t51140069
Download citation file:
2022 ASM International Catalog: Issue 1
View new, upcoming, and best-selling ASM Handbooks, technical books, and databases.