Skip Nav Destination
ASM Technical Books
Corrosion of Weldments
Edited by
ASM International
ISBN electronic:
978-1-62708-339-3
Publication date:
2006
Book Chapter
Chapter 10: Weld Corrosion in Specific Industries and Environments
-
Published:2006
Abstract
This chapter reviews weld corrosion in three key application areas: petroleum refining and petrochemical operations, boiling water reactor piping systems, and components used in pulp and paper plants. The discussion of each area addresses general design and service characteristics, types of weld corrosion issues, and prevention or mitigation strategies.
Topics
Corrosion,
Weld corrosion,
Hydrogen embrittlement,
Heat-affected zone,
Steel,
Boiling water reactors,
Residual stress analysis,
Nickel alloys,
Zirconium alloys,
Microstructural analysis,
Welding,
Chemical composition,
Weldability,
Nondestructive testing,
Electrochemical corrosion testing,
Process piping,
Digesters,
Chemical and petrochemical processing equipment,
Oil and gas refining equipment,
Pulp and paper processing equipment
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Weld Corrosion in Specific Industries and Environments, Corrosion of Weldments, Edited By J. R. Davis, ASM International, 2006, p 177–202, https://doi.org/10.31399/asm.tb.cw.t51820177
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Basic Understanding of Weld Corrosion
Corrosion of Weldments
Corrosion of Duplex Stainless Steel Weldments
Corrosion of Weldments
Corrosion of Carbon Steel and Low-Alloy Steel Weldments
Corrosion of Weldments
Corrosion of Martensitic Stainless Steel Weldments
Corrosion of Weldments
Corrosion of Nonferrous Alloy Weldments
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion of High-Nickel Alloy Weldments
Corrosion of Weldments
Corrosion of Dissimilar Metal Weldments
Corrosion of Weldments
Corrosion of Nonferrous Alloy Weldments
Corrosion of Weldments