Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications
Chapter 15: Selection of Materials for Tribosystems
-
Published:2021
Abstract
This chapter provides guidelines and insights on the selection of materials, coatings, and treatments for friction and wear applications. It begins with a review of the system nature of tribological effects, the subtleties of friction, and the selection idiosyncrasies of the material systems and lubricants covered in prior chapters. It then presents a systematic approach for selecting tribomaterials, using an automotive fan motor as an example.
Selection of Materials for Tribosystems, Tribomaterials: Properties and Selection for Friction, Wear, and Erosion Applications, By Kenneth G. Budinski, Steven T. Budinski, ASM International, 2021, p 421–444, https://doi.org/10.31399/asm.tb.tpsfwea.t59300421
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.