Chapter 8: Magnetic and Physical Properties
-
Published:2007
Abstract
This chapter discusses the advantages of using powder metallurgy to produce magnetic materials, particularly its ability to control chemistry and near-net shape. It also explains how process parameters and powder characteristics influence the physical and magnetic properties of common stainless steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Magnetic and Physical Properties, Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties, By Erhard Klar, Prasan K. Samal, ASM International, 2007, p 131–146, https://doi.org/10.31399/asm.tb.pmsspmp.t52000131
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Electromagnetic and Thermal Properties of Materials
Induction Heating and Heat Treatment
Introduction
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Magnetic Properties
Materials at Low Temperatures
Manufacture and Characteristics of Stainless Steel Powders
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Alloying Elements, Optimal Sintering, and Surface Modification in PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Physical Properties of Metals
Elements of Metallurgy and Engineering Alloys
Compacting and Shaping
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Physical Properties of Cast Irons
Cast Iron Science and Technology
Electromagnetic Problem Solutions
Induction Heating and Heat Treatment