Chapter 6: Alloying Elements, Optimal Sintering, and Surface Modification in PM Stainless Steels Available to Purchase
-
Published:2007
Page range:
101 - 107
Abstract
This chapter describes the most effective ways to improve the corrosion resistance of sintered stainless steels, including increasing alloy content, optimizing the sintering process, and the use of surface treatments and modifications.
You do not currently have access to this chapter.
Citation
Alloying Elements, Optimal Sintering, and Surface Modification in PM Stainless Steels, Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties, By Erhard Klar, Prasan K. Samal, ASM International, 2007, p 101–107, https://doi.org/10.31399/asm.tb.pmsspmp.t52000101
Download citation file:
Related Book Content
Surface Modification Using Energy Beams
Corrosion: Fundamentals, Testing, and Protection
Introduction
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Publication History
Surface Engineering
Foreword
Surface Engineering
Preface
Surface Engineering
Credits
Surface Engineering
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Manufacture and Characteristics of Stainless Steel Powders
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Friction Stir Processing and Surfacing
Friction, Lubrication, and Wear Technology
Magnetic and Physical Properties
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties