Appendix I: Etchants for Revealing Microstructure Available to Purchase
-
Published:1984
Page range:
610 - 711
Abstract
This appendix contains tables that list the composition and capabilities of etchants that reveal the microstructure of metals and alloys, including aluminum, chromium, cobalt, copper, lead, magnesium, molybdenum, nickel, niobium, palladium, platinum, radioactive metals, rare earth metals, rhenium, rhodium, selenium, tellurium, silicon, silver, tantalum, tin, titanium, tungsten, vanadium, and zinc, as well as carbides, oxides, and nitrides.
You do not currently have access to this chapter.
Citation
Etchants for Revealing Microstructure, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 610–711, https://doi.org/10.31399/asm.tb.mpp.t67850610
Download citation file:
Related Book Content
Dislocation Etching Techniques
Metallography Principles and Practice
Atlas of Microstructures
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Etching Methods
Light Microscopy of Carbon Steels
Metallographic Technique: Micrography
Metallography of Steels Interpretation of Structure and the Effects of Processing
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels