Skip Nav Destination
ASM Technical Books
Metallography: Principles and Practice
ASM International
ISBN electronic:
978-1-62708-260-0
Publication date:
1984
Book Chapter
Appendix H: Electrolytic Polishing Solutions
-
Published:1984
Page range:
562 - 609
Abstract
This appendix provides detailed information on the processes and procedures used in electrolytic polishing. It lists important process parameters, including time, temperature, voltage, and current density, as well as the recipes of electrolytic solutions used. The information is presented in tabular form, corresponding to specific metals and their alloys.
You do not currently have access to this chapter.
Citation
Electrolytic Polishing Solutions, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 562–609, https://doi.org/10.31399/asm.tb.mpp.t67850562
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Electromechanical Polishing Procedures
Metallography Principles and Practice
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion: Fundamentals, Testing, and Protection
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Chemical and Electrolytic Polishing
Metallography and Microstructures
Metallographic Practices Generally Applicable to All Metals
Metals Handbook Desk Edition (2nd Edition)
Corrosion Rate Conversion
Corrosion in the Petrochemical Industry (Second Edition)