Appendix C: Macroetchants for Revealing Strain Patterns in Nonferrous Metals
-
Published:1984
Abstract
This appendix lists etch compositions and procedures that reveal strain patterns in aluminum and nickel-base superalloys.
This content is PDF only. Please click on the PDF icon to access.
You do not currently have access to this chapter.
Citation
Macroetchants for Revealing Strain Patterns in Nonferrous Metals, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 536–537, https://doi.org/10.31399/asm.tb.mpp.t67850536
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Fatigue Crack Thresholds
Fatigue and Fracture
Workpiece Materials Database
Metalworking: Bulk Forming
Additive Manufacturing of Nickel-Base Superalloys
Additive Manufacturing Processes
Nickel-Base Alloys: Atlas of Fractographs
Fractography
Nonequilibrium Reactions Precipitation Hardening
Phase Diagrams Understanding the Basics
Modeling of Microstructure Evolution during the Thermomechanical Processing of Nickel-Base Superalloys
Fundamentals of Modeling for Metals Processing
Polycrystalline Cast Superalloys
Properties and Selection: Irons, Steels, and High-Performance Alloys
Aluminum Alloy Temper Designations and Definitions
Properties and Selection of Aluminum Alloys