Abstract
This chapter explains how to achieve accurate, sharp delineation of the microstructure of metals using appropriate etching and contrasting techniques. It covers a variety of methods, including chemical etching, heat tinting, gas contrasting, vapor deposition, magnetic etching, ion bombardment, and dislocation etch pitting.
Microstructure, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 165–266, https://doi.org/10.31399/asm.tb.mpp.t67850165