Metallography: Principles and Practice
Chapter 2: Specimen Preparation for Light Microscopy
-
Published:1984
Abstract
This chapter explains how to prepare metallographic samples for light microscopy and how to anticipate and avoid related problems. It describes standard practices and procedures for sectioning, mounting, grinding, and polishing and identifies common defects along with their causes and cures. It also provides recommendations for handling specific materials and addresses safety concerns.
Sign in
ASM members
Member Sign InSpecimen Preparation for Light Microscopy, Metallography: Principles and Practice, By George F. Vander Voort, ASM International, 1984, p 60–164, https://doi.org/10.31399/asm.tb.mpp.t67850060