Abstract
This appendix provides corrosion rate values for various grades of commercially pure and alloyed titanium. The values were derived from published sources and in-house laboratory tests. These data serve only as a starting point or initial guideline for corrosion performance.
You do not currently have access to this chapter.
Citation
Corrosion Data, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 307–312, https://doi.org/10.31399/asm.tb.ttg2.t61120307
Download citation file:
Related Book Content
Listing of Selected Specification and Standardization Organizations
Titanium: A Technical Guide (Second Edition)
Machining Data
Titanium: A Technical Guide (Second Edition)
Introduction to Titanium and Its Alloys
Heat Treating of Nonferrous Alloys
Machining and Chemical Shaping of Titanium
Titanium Physical Metallurgy, Processing, and Applications
Powder Metallurgy
Titanium: A Technical Guide (Second Edition)
Additive Manufacturing of Titanium and Titanium Alloy Biomedical Devices
Additive Manufacturing in Biomedical Applications
Titanium
Elements of Metallurgy and Engineering Alloys
Heat Treating of Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Deformation and Recrystallization of Titanium and Its Alloys
Heat Treating of Nonferrous Alloys
Properties, Compositions, and Applications of Selected Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)