Appendix B6: Beta and Near-Beta Titanium Alloy Datasheets[1] Available to Purchase
-
Published:2000
Abstract
This appendix provides datasheets describing the chemical composition, processing characteristics, mechanical and fabrication properties, and heat treating of beta and near-beta titanium alloys. Datasheets are provided for the following alloys: Ti-11.5Mo-6Zr-4.5Sn (UNS R58030, Beta III); Ti-3Al-8V-6Cr-4Mo-4Zr (UNS R58640, Beta C and 38-6-44); Ti-10V-2Fe-3Al (Ti-10-2-3); Ti-13V-11Cr-3Al (UNS R58010, Ti-13-11-3); Ti-15V-3Al-3Cr-3Sn (Ti-15-3); Ti-15Mo-3Al-2.7Nb-0.25Si (UNS R58210, TiMetal 21S and Beta 21S); Ti-5Al-2Sn-4Zr-4Mo-2Cr-1Fe (Beta CEZ); Ti-8Mo-8V-2Fe-3Al (Ti-8823); Ti-15Mo-5Zr; Ti-15Mo-5Zr-3Al; Ti-11.5V-2Al-2Sn-11Zr (T129); Ti-12V-2.5Al-2Sn-6Zr (T134); Ti-13V-2.7Al-7Sn-2Zr (T175); Ti-8V-5Fe-1Al; and Ti-16V-2.5Al.
Beta and Near-Beta Titanium Alloy Datasheets, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 240–282, https://doi.org/10.31399/asm.tb.ttg2.t61120240