Abstract
This appendix provides datasheets describing the chemical composition, processing characteristics, mechanical and fabrication properties, and heat treating of alpha and near-alpha titanium alloys. Datasheets are provided for the following alloys: Ti-3Al-2.5V (ASTM Grade 9, UNS R56320), Ti-5Al-2.5Sn (UNS R54520/R54521), Ti-6Al-2Nb-1Ta-0.8Mo (UNS R56210), Ti-6Al-2Sn-4Zr-2Mo-0.08Si (UNS R54620), Ti-8Al-1Mo-1V (UNS R54810), and Ti-6Al-2.75Sn-4Zr-0.4Mo-0.45Si (Ti-1100).
You do not currently have access to this chapter.
Citation
Alpha and Near-Alpha Titanium Alloy Datasheets, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 159–194, https://doi.org/10.31399/asm.tb.ttg2.t61120159
Download citation file:
Related Book Content
Alpha-Beta Titanium Alloy Datasheets
Titanium: A Technical Guide (Second Edition)
Beta and Near-Beta Titanium Alloy Datasheets
Titanium: A Technical Guide (Second Edition)
Principles of Alloying Titanium
Titanium Physical Metallurgy, Processing, and Applications
Mechanical Properties and Testing of Titanium Alloys
Titanium Physical Metallurgy, Processing, and Applications
Modeling and Simulation of Texture Evolution during the Thermomechanical Processing of Titanium Alloys
Fundamentals of Modeling for Metals Processing
Brazing of Refractory and Reactive Metals
Welding, Brazing, and Soldering
Welding of Titanium Alloys
Welding, Brazing, and Soldering
Superalloys for High Temperatures—a Primer
Superalloys: A Technical Guide (Second Edition)
Compositions of Standard Carbon Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Compositions of Standard Alloy Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels