Abstract
This appendix contains several tables listing UNS numbers, common names, and descriptions of important titanium alloys and where they are typically used.
Topics
Microstructure,
Corrosion,
Cast product forms,
Titanium powder,
Wrought product forms,
Titanium alloys,
Casting,
Conversion coating,
Plating,
Heat treatment,
Welding,
Machining,
Forging,
Forming,
Powder metallurgy,
Surface treatment,
Alloy composition,
Machinability,
Mechanical properties,
Physical properties,
Materials selection,
Titanium-matrix composites,
Phase diagrams,
Time-temperature transformation diagram
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Summary Table of Titanium Alloys, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 139–141, https://doi.org/10.31399/asm.tb.ttg2.t61120139
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Titanium Alloy Datasheets Introduction
Titanium: A Technical Guide (Second Edition)
Cross Reference to Equivalent Titanium Alloys
Titanium: A Technical Guide (Second Edition)
Stress-Corrosion Cracking of Titanium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Listing of Selected Specification and Standardization Organizations
Titanium: A Technical Guide (Second Edition)
Introduction to Selection of Titanium Alloys
Titanium: A Technical Guide (Second Edition)
Forging and Forming
Titanium: A Technical Guide (Second Edition)
Corrosion Data
Titanium: A Technical Guide (Second Edition)
Machining Data
Titanium: A Technical Guide (Second Edition)
Forming of Titanium Plate, Sheet, Strip, and Tubing
Titanium Physical Metallurgy, Processing, and Applications
Titanium and Titanium Alloys
Alloying Understanding the Basics