Titanium castings are used in a wide range of aerospace, chemical process, marine, biomedical, and automotive applications. This chapter provides an overview of titanium casting and associated processes and how they compare with other manufacturing methods. It also discusses the role heat treating and its effect on the tensile properties of different titanium alloys.