Titanium: A Technical Guide (Second Edition)Available to Purchase
Titanium: A Technical Guide, Second Edition provides a review of the significant features of the metallurgy and application of titanium and its alloys. All technical aspects of the use of titanium are covered, with sufficient metals property data. The book begins with an introduction and then covers selection of titanium alloys, metallurgy of titanium, ingot metallurgy and mill products, forging and forming, castings, powder metallurgy, heat treating, joining, machining, cleaning and finishing, properties, and corrosion resistance. Appendices include additional reference tables and datasheets for the most important commercial grades of titanium and titanium alloys. For information on the print version, ISBN: 978-0-87170-749-9, follow this link.