Most integrated titanium mills have primary working equipment designed specifically for titanium. This chapter describes the forging, rolling, and extruding equipment used to produce titanium mill products and sheds light on the corresponding process, structure, property relationships.
Topics
Deformation structures,
Microstructure,
Corrosion,
Heat exchangers,
Pressure vessels,
Compressors,
Orthopedic implants,
Bicycle forks and frames,
Titanium alloys,
Casting,
Metallography,
Joining,
Machining,
Extrusion,
Forging,
Forming,
Powder metallurgy,
Mechanical properties,
Shafts,
Distillation columns,
Medical instruments,
Surgical screws,
Submersibles,
Binary phase diagram,
Phase transformations,
Solidification,
Wrought product forms,
Rolling
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Primary Working, Titanium: Physical Metallurgy, Processing, and Applications, Edited By F.H. Froes, ASM International, 2015, p 207–223, https://doi.org/10.31399/asm.tb.tpmpa.t54480207
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Glossary: Bulk Forming
Metalworking: Bulk Forming
Metalworking
Beryllium Chemistry and Processing
Deformation Processing
Elements of Metallurgy and Engineering Alloys
Bulk Deformation
Metals Fabrication Understanding the Basics
Secondary Working of Bar and Billet
Titanium Physical Metallurgy, Processing, and Applications
Corrosion Resistance of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Beryllium and Aluminum-Beryllium Alloys
Powder Metallurgy
Cold Welding
Welding Fundamentals and Processes
Primary Mill Fabrication
Metals Fabrication Understanding the Basics
Research and Development
Aluminum Extrusion Technology