Abstract
This chapter discusses the use of nondestructive inspection methods, including visual, ultrasonic, radiographic, and thermographic techniques, and the types of flaws and damages they can reveal in composite parts and assemblies. It describes the basic principles behind each method along with best practices and procedures.
Topics
Environmental degradation,
Adhesion testing,
Composites products and forms,
Composite processing,
Adhesive bonding,
Mechanical fastening,
Nondestructive testing,
Materials selection,
Structural analysis,
Ceramic-matrix composites,
Sandwich structures,
Ceramic matrices,
Metallic matrices,
Organic matrices,
Aluminum-matrix composites,
Titanium-matrix composites,
Polymer-matrix composites,
Fibers,
Fiber-reinforced composites,
Industrial radiography,
Thermography,
Ultrasonic inspection,
Visual inspection
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Nondestructive Inspection, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 333–350, https://doi.org/10.31399/asm.tb.scm.t52870333
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Inspection of Forgings
Inspection of Metals Understanding the Basics
Inspection of Weldments and Brazed Assemblies
Inspection of Metals Understanding the Basics
Nondestructive Inspection of Cast Irons
Cast Iron Science and Technology
Inspection of Tubular Products
Inspection of Metals Understanding the Basics
Inspection, Data Collection, and Management
Corrosion: Environments and Industries
Inspection of Steel Bar and Wire
Inspection of Metals Understanding the Basics
Inspection of Castings
Inspection of Metals Understanding the Basics
Nondestructive Inspection of Adhesive-Bonded Joints
Nondestructive Evaluation of Materials