Chapter 7: Processing Science of Polymer Matrix Composites
-
Published:2010
Abstract
This chapter provides an overview of the tools and techniques, as well as some of the underlying theory, that have proven useful for process modeling and simulation. It begins by presenting the framework of a thermoset cure model that accounts for kinetics, viscosity, heat transfer, flow, voids, and residual stress. It then discusses each variable in detail, explaining how it affects the cure process, how it is measured, and how it can be expressed mathematically in the form of a simple model. The discussions throughout the chapter are supported by numerous images, diagrams, and data plots.
Sign in
ASM members
Member Sign InProcessing Science of Polymer Matrix Composites, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 201–234, https://doi.org/10.31399/asm.tb.scm.t52870201
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.