Abstract
This chapter familiarizes readers with the many and varied thermoset composite fabrication processes and the types of applications for which they were developed. It describes wet lay-up, prepreg lay-up, and low-temperature vacuum bag curing prepreg processes, which are best suited for low-volume, medium-sized and larger parts. It also discusses filament winding and preforming processes (including weaving, knitting, stitching, and braiding) in addition to resin-transfer molding, resin film infusion, and pultrusion.
You do not currently have access to this chapter.
Citation
Thermoset Composite Fabrication Processes, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 119–182, https://doi.org/10.31399/asm.tb.scm.t52870119
Download citation file:
Related Book Content
Thermoplastic Composites Manufacturing
Composites
Phenolic Resins
Composites
Design Guidelines
Composites
Introduction—Composite Materials and Optical Microscopy
Metallography and Microstructures
Vacuum Infusion
Composites
Glossary of Filament-Winding Terms
Composite Filament Winding
Resin Transfer Molding and Structural Reaction Injection Molding
Engineered Materials Handbook Desk Edition
Pultrusion
Composites
Bismaleimide Resins
Composites
Joining of Organic-Matrix Composites
Welding, Brazing, and Soldering