Appendix 5: Tempering Curves
-
Published:2015
Abstract
This appendix provides tempering curves for common grades of steel, including 1045, 1144, 4140, 4150, and E52100.
Topics
Hardness testing,
Induction furnaces,
Quenchants,
Quenching,
Induction surface hardening,
Case hardening,
Through hardening,
Induction tempering,
Hardenability,
Eddy current inspection,
Magnetic particle inspection,
Surface hardness,
Liquid penetrant inspection,
Ultrasonic inspection,
Inspection,
Qualification,
Statistical quality control,
Steel,
Tempering,
Hardness,
Temperature
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Tempering Curves, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 343–345, https://doi.org/10.31399/asm.tb.piht2.t55050343
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Temperature Measurement
Steel Metallurgy for the Non-Metallurgist
Austenitizing and Typical Heat Treatment Temperatures for Steels
Heat Treating of Irons and Steels
Temperature and Heat Transfer
Cold and Hot Forging Fundamentals and Applications
Elastic Properties
Materials at Low Temperatures
Temperature Conversions
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Hardenability Curves
Practical Induction Heat Treating (Second Edition)
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels