Appendix 5: Tempering Curves
-
Published:2015
Page range:
343 - 345
Abstract
This appendix provides tempering curves for common grades of steel, including 1045, 1144, 4140, 4150, and E52100.
You do not currently have access to this chapter.
Citation
Tempering Curves, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 343–345, https://doi.org/10.31399/asm.tb.piht2.t55050343
Download citation file:
Related Book Content
Temperature Measurement
Steel Metallurgy for the Non-Metallurgist
Austenitizing and Typical Heat Treatment Temperatures for Steels
Heat Treating of Irons and Steels
Hardenability Curves
Practical Induction Heat Treating (Second Edition)
Temperature and Heat Transfer
Cold and Hot Forging Fundamentals and Applications
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
Temperature Conversions
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Elastic Properties
Materials at Low Temperatures