Book Chapter
Chapter 12: Standards and Inspection
-
Published:2015
Page range:
245 - 262
Abstract
This chapter discusses the methods and procedures used for inspecting induction-hardened parts. It provides information on hardness and case depth measurements, nondestructive testing and surface analysis, the effect of various hardening errors, and relevant test standards.
You do not currently have access to this chapter.
Citation
Standards and Inspection, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 245–262, https://doi.org/10.31399/asm.tb.piht2.t55050245
Download citation file:
Related Book Content
Principles of Induction Hardening and Inspection
Induction Heating and Heat Treatment
Inspection and NDT Methods
Induction Heating and Heat Treatment
Testing and Inspection of Metals—The Quest for Quality
Metallurgy for the Non-Metallurgist (Second Edition)
Induction Case Hardening of Axle Shafts
Induction Heating and Heat Treatment
Inspection Methods: Overview and Comparison
Inspection of Metals Understanding the Basics
Postcoating Operations
Thermal Spray Technology
Surface Hardening of Steel
Practical Heat Treating: Processes and Practices
Induction Hardening of Gears and Gear-Like Components
Induction Heating and Heat Treatment
Carbonitriding
Practical Heat Treating: Processes and Practices
Cracked Aircraft Wing Spar
ASM Failure Analysis Case Histories: Air and Spacecraft