Cast irons, like steels, are iron-carbon alloys but with higher carbon levels than steels to take advantage of eutectic solidification in the binary iron-carbon system. Like steel, heat treatment of cast iron includes stress relieving, annealing, normalizing, through hardening, and surface hardening. This chapter introduces solid-state heat treatment of iron castings, covering general considerations for heat treatment and discussing the processes, advantages, and disadvantages of heat treatment of cast iron.
Heat Treatment of Cast Irons, Practical Heat Treating: Basic Principles, By Jon L. Dossett, ASM International, 2020, p 331–350, https://doi.org/10.31399/asm.tb.phtbp.t59310331