Mechanics and Mechanisms of Fracture: An Introduction
Chapter 3: Fatigue Strength of Metals
-
Published:2005
Abstract
This chapter examines the stress-strain characteristics of metals and alloys subjected to cyclic loading and the cumulative effects of fatigue. It begins by explaining how a single load reversal can lower the yield stress of a material and how repeated reversals can cause strain hardening and softening, both of which lead to premature failure. It then discusses the stages of fatigue fracture, using detailed images to show how cracks initiate and grow and how they leave telltale marks on fracture surfaces. It goes on to describe fatigue life assessment methods and demonstrate their use on different metals and alloys....
Sign in
ASM members
Member Sign InFatigue Strength of Metals, Mechanics and Mechanisms of Fracture: An Introduction, By Alan F. Liu, ASM International, 2005, p 121–167, https://doi.org/10.31399/asm.tb.mmfi.t69540121
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.