Appendix 3: Temper Designations for Aluminum and Aluminum Alloys
-
Published:1999
Abstract
This appendix provides information on temper designations for strain-hardened aluminum, heat treatable aluminum alloys, and annealed aluminum products.
Topics
Aqueous corrosion,
Atmospheric corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Erosion corrosion,
Galvanic corrosion,
Intergranular corrosion,
Weld corrosion,
Stray current corrosion,
Corrosion fatigue,
Stress corrosion cracking,
Corrosion inhibitors,
Cast aluminum alloys,
Wrought aluminum alloys,
Aluminum alloys,
Anodizing,
Cladding,
Chromate conversion coating,
Plating,
Cleaning,
Alloy composition,
Corrosion testing,
Aluminum-matrix composites,
Annealing,
Aluminum
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Temper Designations for Aluminum and Aluminum Alloys, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 265–268, https://doi.org/10.31399/asm.tb.caaa.t67870265
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Aluminum Alloy Nomenclature and Temper Designations
Heat Treating of Nonferrous Alloys
Deformation and Recrystallization of Titanium and Its Alloys
Titanium Physical Metallurgy, Processing, and Applications
Annealing of Aluminum and Its Alloys
Heat Treating of Nonferrous Alloys
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Aluminum—The Light Metal
The History of Metals in America
Understanding the Corrosion Behavior of Aluminum
Corrosion of Aluminum and Aluminum Alloys
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys