Appendix 2: Compositions of Cast Aluminum and Aluminum Alloys
-
Published:1999
Abstract
This appendix includes composition limit data for aluminum castings and ingots.
Topics
Aqueous corrosion,
Atmospheric corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Erosion corrosion,
Galvanic corrosion,
Intergranular corrosion,
Weld corrosion,
Stray current corrosion,
Corrosion fatigue,
Stress corrosion cracking,
Corrosion inhibitors,
Cast aluminum alloys,
Wrought aluminum alloys,
Aluminum alloys,
Anodizing,
Cladding,
Chromate conversion coating,
Plating,
Cleaning,
Alloy composition,
Corrosion testing,
Aluminum-matrix composites,
Ingots,
Chemical composition
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Compositions of Cast Aluminum and Aluminum Alloys, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 259–264, https://doi.org/10.31399/asm.tb.caaa.t67870259
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Glossary of Terms
Aluminum Alloy Castings Properties, Processes, and Applications
Introduction
Corrosion of Aluminum and Aluminum Alloys
Aluminum Alloy Nomenclature and Temper Designations
Heat Treating of Nonferrous Alloys
Aluminum and Aluminum Alloys
Alloying Understanding the Basics
Melting and Melt Treatment of Aluminum Alloys
Aluminum Science and Technology
Temperature Requirements for Heating Titanium, Aluminum, Magnesium, and Copper Alloys
Induction Heating and Heat Treatment
Cast Ingot Cracked During Forging
ASM Failure Analysis Case Histories: Processing Errors and Defects
An Example of Decarburization in Alloy Steels and Its Effect on Further Processing
ASM Failure Analysis Case Histories: Processing Errors and Defects
Ingot Metallurgy and Mill Products
Titanium: A Technical Guide (Second Edition)
Casting of Beryllium
Beryllium Chemistry and Processing