Abstract
This chapter explains how mechanical processes, including erosion, cavitation, impingement, and fretting, contribute to the effects of corrosion in aluminum alloys. It describes the two main types of erosion-corrosion and the factors involved in cavitation and liquid impingement erosion along with testing and prevention methods. It also provides information on fretting corrosion and fretting fatigue.
Topics
Aqueous corrosion,
Atmospheric corrosion,
Crevice corrosion,
Microbiologically-influenced corrosion,
Pitting corrosion,
Erosion corrosion,
Galvanic corrosion,
Intergranular corrosion,
Weld corrosion,
Stray current corrosion,
Corrosion fatigue,
Stress corrosion cracking,
Corrosion inhibitors,
Cast aluminum alloys,
Wrought aluminum alloys,
Aluminum alloys,
Anodizing,
Cladding,
Chromate conversion coating,
Plating,
Cleaning,
Alloy composition,
Corrosion testing,
Aluminum-matrix composites,
Cavitation corrosion,
Fretting corrosion,
Liquid impingement erosion,
Cavitation erosion testing,
Aluminum
You do not currently have access to this chapter.
Citation
Erosion, Cavitation, Impingement, and Fretting Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 85–97, https://doi.org/10.31399/asm.tb.caaa.t67870085
Download citation file:
Related Book Content
Effects of Metallurgical Variables on the Corrosion of Aluminum Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion
Elements of Metallurgy and Engineering Alloys
Aluminum—The Light Metal
The History of Metals in America
Summary of Aluminum Temper Designations
Aluminum Science and Technology
Laser Beam Machining of Aluminum and Aluminum Alloys
Aluminum Science and Technology
Chemical and Electrolytic Brightening
Aluminum Science and Technology
Understanding the Corrosion Behavior of Aluminum
Corrosion of Aluminum and Aluminum Alloys
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys
Chemical Compositions and International Designations for Aluminum Alloys
Metals Handbook Desk Edition (2nd Edition)
Etching of Aluminum and Its Alloys
Aluminum Science and Technology