Corrosion of Aluminum and Aluminum Alloys
Chapter 5: Galvanic, Deposition, and Stray-Current Corrosion
-
Published:1999
Abstract
This chapter discusses three related corrosion mechanisms, galvanic, deposition, and stray-current corrosion, explaining why they occur and how they affect the corrosion process. It includes information on testing and prevention methods along with examples of the type of damage associated with these corrosion mechanisms.
Galvanic, Deposition, and Stray-Current Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 75–83, https://doi.org/10.31399/asm.tb.caaa.t67870075