Corrosion of Aluminum and Aluminum Alloys
Chapter 1: Introduction
-
Published:1999
Abstract
Aluminum is the second most widely used metal in the world. It is readily available, offers a wide range of properties, and can be shaped, coated, and joined using a variety of methods. This chapter discusses some of the key attributes of wrought and cast aluminum alloys and the classifications, designations, and grades of available product forms. It also explains how aluminum alloys are used in aerospace, automotive, rail, and marine applications as well as in building and construction, electrical products, manufacturing equipment, packaging, and consumer durables such as appliances and furniture.
Sign in
ASM members
Member Sign InIntroduction, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 1–24, https://doi.org/10.31399/asm.tb.caaa.t67870001
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.