Lightweight Materials: Understanding the Basics
Chapter 12: Selection Guidelines for Lightweight Materials
-
Published:2012
Abstract
This chapter consists of three parts. The first part provides data and guidelines for selecting materials and processing routes. It compares the basic properties of metals, ceramics, and polymers, identifies important measures of performance, and discusses manufacturing processes and their compatibility with specific materials. The chapter then presents general guidelines for selecting lightweight materials, and concludes with a review of lightweight metals, plastics, and composites used in automotive applications.
Sign in
ASM members
Member Sign InSelection Guidelines for Lightweight Materials, Lightweight Materials: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 621–672, https://doi.org/10.31399/asm.tb.lmub.t53550621
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.