Titanium aluminides are lightweight materials that have relatively high melting points and good high-temperature strength. They also tend to be stronger and lighter than conventional titanium alloys, but considerably less ductile. This chapter begins with a review of the titanium-aluminum phase diagram, focusing on the properties, compositions, and microstructures of alpha-2 Ti3Al alloys. It then describes the properties, microstructures, and compositions of orthorhombic, gamma, and near-gamma alloys as well as the processing methods and procedures normally used in their production.