Appendix 2: Chemical Compositions of Alloys and Filler Metals Available to Purchase
-
Published:2007
Page range:
445 - 453
Abstract
This appendix is a collection of tables listing the chemical compositions of wrought ferritic steels; wrought stainless steels; cast corrosion- and heat-resistant alloys; wrought iron-, nickel-, and cobalt-base alloys; cast nickel- and cobalt-base alloys; oxide-dispersion-strengthened alloys; and iron-, nickel- and cobalt-base filler metals.
You do not currently have access to this chapter.
Citation
Chemical Compositions of Alloys and Filler Metals, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 445–453, https://doi.org/10.31399/asm.tb.htcma.t52080445
Download citation file:
Related Book Content
Cobalt and Cobalt Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Hot Corrosion in Gas Turbines
High-Temperature Corrosion and Materials Applications
Effects of Metallurgical Variables on the Corrosion of High-Nickel Alloys
Corrosion in the Petrochemical Industry (Second Edition)
Brazing of Heat-Resistant Alloys, Low-Alloy Steels, and Tool Steels
Welding, Brazing, and Soldering
Nickel and Nickel Alloys
Metals Handbook Desk Edition (2nd Edition)
Arc Welding
Metals Handbook Desk Edition (2nd Edition)
Effects of Metallurgical Variables on the Corrosion of High-Nickel Alloys
Corrosion: Fundamentals, Testing, and Protection
Forging of Heat-Resistant Alloys
Metalworking: Bulk Forming
Diffusion Brazing
Principles of Brazing
Heat Treatment of Cobalt-Base Alloys
Heat Treating of Nonferrous Alloys