Abstract
This chapter discusses material-related problems associated with coal-fired burners. It explains how high temperatures affect heat-absorbing surfaces in furnace combustion areas and in the convection pass of superheaters and reheaters. It describes how low-NOx combustion technology, intended to reduce NOx emissions, accelerates tube wall wastage. It also covers circumferential cracking in furnace waterwalls, thermal fatigue cracking induced by waterlances and water cannons, superheater-reheater corrosion, and erosion in fluidized-bed boilers.
You do not currently have access to this chapter.
Citation
Coal-Fired Boilers, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 259–320, https://doi.org/10.31399/asm.tb.htcma.t52080259
Download citation file:
Related Book Content
Hydrogen Attack
High-Temperature Corrosion and Materials Applications
Erosion and Erosion-Corrosion
High-Temperature Corrosion and Materials Applications
Corrosion Failures in Gas Turbine Hot Components
Handbook of Case Histories in Failure Analysis
Erosive Wear Failures
Failure Analysis and Prevention (2021 Edition)
Corrosion Control by Proper Design
Corrosion: Understanding the Basics
Wear Failures
Fatigue and Fracture Understanding the Basics
Corrosion Resistance of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
Materials Selection for Corrosion Control
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion of Titanium and Titanium Alloys
Corrosion: Materials
Corrosion of Steam Turbines
Corrosion: Environments and Industries