Chapter 5: Carburization and Metal Dusting
-
Published:2007
Page range:
97 - 145
Abstract
This chapter discusses the conditions under which carburization and metal dusting occur. It describes the chemical reactions and thermodynamic relationships that drive carburization and metal dusting attack and the factors that determine the amount of damage that metals and alloys are likely to sustain. The chapter also explains how carburization affects creep strength and fracture toughness, and how surface conditions and finish and the presence of sulfur affect metal dusting behaviors.
You do not currently have access to this chapter.
Citation
Carburization and Metal Dusting, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 97–145, https://doi.org/10.31399/asm.tb.htcma.t52080097
Download citation file:
Related Book Content
Corrosion in High-Temperature Environments
Corrosion: Environments and Industries
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention
Thermodynamics in Extrusion
Aluminum Extrusion Technology
Case of Metal Dusting on HK40 HyL III Radiant Pipe Heat Exchanger
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Thermal Expansion
Materials at Low Temperatures
Electrochemical Thermodynamics: The Gibbs Function, Electrochemical Reactions, and Equilibrium Potentials
Fundamentals of Electrochemical Corrosion
Thermodynamics of Extraction
Beryllium Chemistry and Processing
Thermodynamics of Microstructure Change
Thermodynamics of Microstructures
Failure of a Transfer Line on an Ethane Cracking Furnace Due to Sulfidation
ASM Failure Analysis Case Histories: Oil and Gas Production Equipment
Thermodynamics of Interfaces
Thermodynamics of Microstructures