Fundamentals of Electrochemical Corrosion
Chapter 4: Kinetics of Coupled Half-Cell Reactions
-
Published:2000
Abstract
This chapter develops a corrosion model that accounts for solution potentials and the effects of coupling between cathodic and anodic reactions. It begins by examining potential differences at various points (in the solution) along a path from the anode to the cathode area. It then presents a simple model of a galvanically coupled electrode, in which the metal is represented as an array of anode and cathode reaction surfaces. The chapter goes on to develop the related theory of mixed electrodes, showing how it can be used to predict corrosion rates based on measured potentials and current densities, polarization...
Sign in
ASM members
Member Sign InKinetics of Coupled Half-Cell Reactions, Fundamentals of Electrochemical Corrosion, By E.E. Stansbury, R.A. Buchanan, ASM International, 2000, p 127–181, https://doi.org/10.31399/asm.tb.fec.t65940127
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!