The nose bullet of an aircraft engine developed a crack and was removed and examined to determine the cause. The bullet was made from a titanium alloy and was of welded construction. Close-up views show that the crack originated in an area of rework along the weld seam and propagated on either side. The case is a reminder that rework in a welded region requires careful planning and thought.