Failure Analysis of Engineering Structures: Methodology and Case Histories
Case 18: Failure of a Tail Rotor Blade in a Helicopter
-
Published:2005
Abstract
A helicopter lost the outboard rib on a tail rotor blade in flight and was forced to land because of the resulting vibrations. The investigation that followed is described in this chapter along with key findings. As shown in a sketch, the rib is held in place by a set of six rivets. All of the rivets on the failed blade were missing and sections of skin were torn from most of the rivet holes. One such rivet hole was examined in a SEM, revealing corrosion on one of the tear surfaces and dimples (characteristic of ductile overload failure)...
Sign in
ASM members
Member Sign InFailure of a Tail Rotor Blade in a Helicopter, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 107–109, https://doi.org/10.31399/asm.tb.faesmch.t51270107
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.