Case 10: Failure of a Wheel Hub in an Aircraft Available to Purchase
-
Published:2005
Page range:
84 - 86
Abstract
An aircraft tire burst while inflating, causing one of the flanges on the wheel hub to fracture. This chapter provides a summary of the investigation along with key findings. It includes images of the damaged hub and describes how various parts failed as the pressure in the tire increased. It explains that the hub material was of good quality under uniform load and that it fractured quickly by cleavage due to the force exerted by the overinflated tire.
You do not currently have access to this chapter.
Citation
Failure of a Wheel Hub in an Aircraft, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 84–86, https://doi.org/10.31399/asm.tb.faesmch.t51270084
Download citation file:
Related Book Content
Failure of a Main Wheel Bearing Housing Flange in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Tie-Rod in an Aircraft Towing Tractor
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Aircraft Engine Compressor Rotors
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Stabilizer Link Rod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Wing Control Cable in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of an Adaptor Assembly in an Electronic Pod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Main Undercarriage Struts in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Second-Stage Turbine Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a First-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Second-Stage Compressor Blade in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories