Case 9: Failure of a Tail Rotor Blade in a Helicopter
-
Published:2005
Page range:
82 - 83
Abstract
This chapter discusses the investigation of a helicopter tail rotor blade that fractured during a test flight. It includes images of the damaged blade along with close-ups of both sides of the blade tip showing that the tip tore off at the rivets. Based on their observations, investigators concluded that the rotor blade encountered a foreign object in flight causing the tip to shear off.
You do not currently have access to this chapter.
Citation
Failure of a Tail Rotor Blade in a Helicopter, Failure Analysis of Engineering Structures: Methodology and Case Histories, By V. Ramachandran, A.C. Raghuram, R.V. Krishnan, S.K. Bhaumik, ASM International, 2005, p 82–83, https://doi.org/10.31399/asm.tb.faesmch.t51270082
Download citation file:
Related Book Content
Failure of a Tail Rotor Blade in a Helicopter
Failure Analysis of Engineering Structures Methodology and Case Histories
Cracking in a Tail Rotor Blade in a Helicopter
Failure Analysis of Engineering Structures Methodology and Case Histories
Fatigue Fracture of a Sand-Cast Steel Axle Housing That Originated at a Hot Tear
ASM Failure Analysis Case Histories: Automobiles and Trucks
Failure of a Main Wheel Bearing Housing Flange in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Stabilizer Link Rod in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Fuel Nozzle in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Wing Control Cable in an Aircraft
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of a Fourth-Stage Compressor Disc in an Aircraft Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Failure of Connecting Rod Bolts in a Ground-Based Engine
Failure Analysis of Engineering Structures Methodology and Case Histories
Mode III Fatigue Crack Growth Following the Curvature of the Heat-Affected Zone of a Type 321 Stainless Steel Spot Weld
Handbook of Case Histories in Failure Analysis