This chapter discusses the basic steps of a failure investigation. It explains that the first step is to gather and document information about the failed component and its operating history. It advises investigators to visit the failure site as soon as possible to record damages and collect test specimens for subsequent examination and chemical analysis. It also discusses the role of mechanical property testing, the use of nondestructive evaluation, and the final step of generating a report.