Inspection of Metals: Understanding the BasicsAvailable to Purchase
Edited by
ASM International
ISBN electronic:
978-1-62708-305-8
Publication date:
2013
Book Chapter
Chapter 1: Inspection Methods: Overview and Comparison Available to Purchase
-
Published:2013
Page range:
1 - 20
Abstract
This chapter provides an overview of the various inspection methods used with metals and alloys, namely visual inspection, coordinate measuring machines, machine vision, hardness testing, tensile testing, chemical analysis, metallography, and nondestructive testing. The nondestructive testing methods discussed are liquid penetrant inspection, magnetic particle inspection, eddy current inspection, radiographic inspection, and ultrasonic testing.
You do not currently have access to this chapter.
Citation
Inspection Methods: Overview and Comparison, Inspection of Metals: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2013, p 1–20, https://doi.org/10.31399/asm.tb.imub.t53720001
Download citation file:
Related Book Content
Testing and Inspection of Metals—The Quest for Quality
Metallurgy for the Non-Metallurgist (Second Edition)
Machine Vision and Robotic Inspection Systems
Nondestructive Evaluation of Materials
Standards and Inspection
Practical Induction Heat Treating (Second Edition)
Systematic Examination
Systematic Analysis of Gear Failures
Machine Vision
Inspection of Metals Understanding the Basics
Glossary of Terms
Tensile Testing (Second Edition)
Overview of the Mechanisms of Failure in Heat Treated Steel Components
Failure Analysis of Heat Treated Steel Components
Tensile Testing of Elastomers
Tensile Testing (Second Edition)