Abstract
When a material is sintered and evaluated for performance, the primary focus is on mechanical properties. This chapter discusses structural properties for representative materials. Some guidelines are presented on the types of tests and how property values depend on the testing procedure. Mechanical hardness and strength tabulations are provided to document sintered properties.
Topics
Grain structure,
Microstructure,
Dimensional distortion,
Polymers,
Binder jetting,
Binder-assisted extrusion,
Cold isostatic pressing,
Injection molding,
Hardness,
Density,
Ceramic-matrix composites,
Metal-matrix composites,
Polymer-matrix composites,
Grain growth,
Sintering,
Mechanical properties,
Performance testing
You do not currently have access to this chapter.
Citation
Component Mechanical Properties, Binder and Polymer Assisted Powder Processing, By Randall M. German, Animesh Bose, ASM International, 2020, p 193–199, https://doi.org/10.31399/asm.tb.bpapp.t59290193
Download citation file:
Related Book Content
Pressed-and-Sintered Ferrous Powder Metallurgy Parts
Metals Handbook Desk Edition (2nd Edition)
Sintering Densification
Binder and Polymer Assisted Powder Processing
Powder Metallurgy
Beryllium Chemistry and Processing
Modeling and Simulation of Press and Sinter Powder Metallurgy
Metals Process Simulation
Binder Jetting and Sintering in Additive Manufacturing
Additive Manufacturing Processes
Sintering and Corrosion Resistance
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Friction Powder Metallurgy Materials
Powder Metallurgy
Sintering of Stainless Steels
Powder Metallurgy
Modeling of Powder Metallurgy Processes
Metals Process Simulation
Vacuum Heat Treating Additively Manufactured Parts
Additive Manufacturing Processes