Chapter 5: Powder-Binder Feedstock Mixing and Testing
-
Published:2020
Abstract
This chapter is a detailed account of various attributes related to mixing and testing of powder-binder feedstocks. Mixing parameters and their effects on feedstock properties is discussed. The attributes reviewed include mixture homogeneity, wetting, powder-binder ratio, feedstock density, elastic modulus, rheological behavior, particle size, formulation control, feedstock mixing, and feedstock properties. The chapter also provides information on the processes involved in feedstock preparation and testing.
Sign in
ASM members
Member Sign InPowder-Binder Feedstock Mixing and Testing, Binder and Polymer Assisted Powder Processing, By Randall M. German, Animesh Bose, ASM International, 2020, p 85–109, https://doi.org/10.31399/asm.tb.bpapp.t59290085
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.