Austenitic Manganese Steels
-
Published:2001
Abstract
This article provides an overview of austenitic manganese steels. It describes the standard composition ranges of commercial products and explains how various alloying elements affect mechanical properties, processing, and performance. The article also discusses special grades of manganese steels and the types of applications for which they have been developed.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Austenitic Manganese Steels, Alloying: Understanding the Basics, Edited By J.R. Davis, ASM International, 2001, p 242–253, https://doi.org/10.31399/asm.tb.aub.t61170242
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Wear-Resistant Austenitic Manganese Steels
Metals Handbook Desk Edition (2nd Edition)
Compacted Graphite Irons
Alloying Understanding the Basics
Hardenability and Heat Treatment
Steel Castings Handbook (Sixth Edition)
Malleable Irons
Alloying Understanding the Basics
High-Alloy White Irons
Alloying Understanding the Basics
High-Strength Low-Alloy Steels
Alloying Understanding the Basics
Maraging Steels
Alloying Understanding the Basics
Titanium and Titanium Alloys
Alloying Understanding the Basics
Zinc and Zinc Alloys
Alloying Understanding the Basics
Cemented Carbides and Cermets
Alloying Understanding the Basics