Metallography of Steels: Interpretation of Structure and the Effects of Processing
Chapter 14: Structural Steels and Steels for Pressure Vessels, Piping, and Boilers
-
Published:2018
Abstract
This chapter discusses the properties and compositions of steels used in pressure vessels, piping, boilers, rebar, and other structural applications. It covers fine-grained steels, quenched and tempered steels, and controlled rolled (thermomechanical treatment) steels. It also compares and contrasts steels used for concrete reinforcement and in various types of pressure vessels, and presents a metallographic study of the effects of welding on the micro and macrostructure of steel.
Sign in
ASM members
Member Sign InStructural Steels and Steels for Pressure Vessels, Piping, and Boilers, Metallography of Steels: Interpretation of Structure and the Effects of Processing, By Hubertus Colpaert;Edited By André Luiz V. da Costa e Silva, ASM International, 2018, p 475–518, https://doi.org/10.31399/asm.tb.msisep.t59220475
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!