Metallography of Steels: Interpretation of Structure and the Effects of Processing
Chapter 13: Advanced Steels for Forming Operations
-
Published:2018
Abstract
This chapter discusses the properties and behaviors of advanced high-strength steels used in the automotive industry, including dual- and complex-phase steels, transformation-induced plasticity steels, ferritic-bainitic steels, and quenched and partitioned steels. It explains how different manufacturing processes, including coating, affect the grain size, microstructure, and formability of these important steels.
Sign in
ASM members
Member Sign InAdvanced Steels for Forming Operations, Metallography of Steels: Interpretation of Structure and the Effects of Processing, By Hubertus Colpaert;Edited By André Luiz V. da Costa e Silva, ASM International, 2018, p 445–474, https://doi.org/10.31399/asm.tb.msisep.t59220445
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!