Abstract
This chapter discusses recycling processes used for metals, plastics, rubber, glass, and paper. Is also describes the advantages of recycled materials.
Topics
Waste handling and recycling
You do not currently have access to this chapter.
Citation
Recycling, Elementary Materials Science, By William R. Hosford, ASM International, 2013, p 149–152, https://doi.org/10.31399/asm.tb.ems.t53730149
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Aluminum Building Products
Aluminum: Technology, Industry, and Applications
Green Coatings
Protective Organic Coatings
Recycling and Other Environmental Considerations for Ceramics and Glasses
Engineered Materials Handbook Desk Edition
Mining, Refining, Smelting, and Recycling
Aluminum: Technology, Industry, and Applications
Hot Chamber Die Casting
Casting
Metal Cutting and Grinding Fluids
Machining