Abstract
This chapter presents guidelines for product designers to choose the best process and alloys while designing a casting. The discussion covers some of the factors pertinent to the selection of the best process for the product function and performance, namely geometric factors, mechanical properties, tooling cost per piece, and overall cost factors. The chapter contains tables listing several markets, products, popular processes, and common alloys and the common processes used for a variety of markets and products.
You do not currently have access to this chapter.
Citation
Process Selection Guidelines, Aluminum Castings Engineering Guide, By Jagan Nath, ASM International, 2018, p 247–252, https://doi.org/10.31399/asm.tb.aceg.t68410247
Download citation file:
Related Book Content
Aluminum Casting Applications
Aluminum Castings Engineering Guide
Product Launch Process
Aluminum Castings Engineering Guide
Introduction
Aluminum Alloy Castings Properties, Processes, and Applications
Dealing with Friction in Design Engineering
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Engineering Design Process Investigation in a Failure Analysis
Analysis and Prevention of Component and Equipment Failures
The Role of the Engineering Expert in Product Liability Litigation
Analysis and Prevention of Component and Equipment Failures
Design and Selection of Plastics Processing Methods
Characterization and Failure Analysis of Plastics
Mechanical Properties Data for Selected Aluminum Alloys
Mechanics and Mechanisms of Fracture An Introduction
Engineering Component Configuration
Aluminum Castings Engineering Guide